Experiment Record Sheet
Experiment Name BYK066N Replacement Test Temperature / Humidity 32/92
Client / Applicant / Experiment Date 26.7.28    
Objective:
The customer uses 60-mesh screen printing for inks. A defoamer is required to match the defoaming performance of BYK066N, with the goal of achieving a bubble-free surface after screen printing.
Formulation
         
Ink binder 100g            
Defoamer BYK066N Anjeka5066N/0.5 Anjeka5066N/0.8 Anjeka 5066N blended with 5088 / 0.5 Anjeka 5066N blended with 5088 / 0.8 Anjeka5052/0.5  
               
               
               
Test Method
Different defoamers were added to 100g of ink binder respectively, and mixed thoroughly at 1000–1500 rpm. The inks were then applied using the customer-provided 60-mesh screen for drawdown testing, with side-by-side comparative evaluation.
 
Test Results
Anjeka 5088 and 5066N showed more noticeable bubbles. Anjeka 5052 and BYK066N exhibited the fewest bubbles after film formation, with comparable performance.
 
BYK066N   BYK066N          
laatste bedrijfscasus over BYK066N Replacement Test laatste bedrijfscasus over BYK066N Replacement Test            
               
               
 
 
Anjeka5052   Anjeka5052          
laatste bedrijfscasus over BYK066N Replacement Test laatste bedrijfscasus over BYK066N Replacement Test            
               
               
Conclusion
Anjeka 5052 can replace BYK066N at an equal dosage. The other formulations are not qualified.